Vous n'avez pas enchéri sur cette enchère.
81.94 CTS ANDAMOOKA MATRIX ROUGH SLABS-SIMILAR PATTERN [BY9481]
- UGS
- Dimensions (mm)
- 40.000 x 26.000 x 6.000mm
- Poids (cts)
- 81.940
- Taper
- Rough
- Couleurs
-
[SAME TREATMENT APPLIES TO FAIRY OPAL]
This is a natural opal treated so it becomes black- We purchase large quanites of rough material and slab it and then treat it so you can get a idea of how it will face. There is a large amount of wastage in preparing this material. You can cut into earrings ring or pendant stones or leave as specimens but you will have to re treat if you take too much away. Check that there isnt another colour bar in the rough you cant expose that may be better than the top.
You may see black spots which is usually blackened sugar which will come off.
Mined in Andamooka Sth Australia
We havve taken the photo of the rough wet!
TREATMENT FOR ANDAMOOKA MATRIX WITH SUGAR ONLY.
MATERIALS
250 grams glucose,white castor sugar,pot or pressure cooker,plastic tweezers.
STEPS
-Pre shape the material
- Thoroughly dry the material in oven sun or hairdryer. You can also soak in aceton for 10 minutes to dry the stones out.
- Put water in pot on low temperature and add glucose and castor sugar. DO NOT BOIL.
-Place warmed stones into warm solution and cover the stone with liquid.
-leave on low temperature for 24 hours but DONT BOIL.
-Remove with tweezers and let cool.Use a paper town to wipe away access.
The next steep is to carbonize the sugar in the stone. Place the stones on a metal or pyrex dish and place in a kiln at 500 F degrees for one hour.This will burn or carbonize the sugar in the stone.
_When the stones have cooled clean on a grinding wheel.
Remember to take all precautions with gloves and mask and clothing with good ventilation.
This is a natural product so results may vary a bit due to how porous the sandstone is. Some material will have to be treated a few times to get good results. You can also experiment with various temperatures as i like to cook with lower temperatures.
Remember to have fun!
WE HAVE TAKEN THE PHOTO WITH THE ROUGH WET.
In the learning section of opal actions there is details on how to treat with acid and sugar but this sugar only gets good results if the material is porous
-
POLISHING
The surface is porous so its hard to get a good finish.
You can polish as a natural stone or coat it with resin to get a better finish.
We suggest a polymer resin as its stable.inert and nontoxic and dosent yellow..Check out our listings of fairy opal polished in sedaopals.Some of there were polished in china under vacume with a amazing finish.
We have also used mono-compontent thermo set resin,cynoacrylates and 2 parts resin but these can turn yellow over time. ive even heard of nail polished used and hardened under uv lights.
The weight and size is app
- UGS
- Dimensions (mm)
- 40.000 x 26.000 x 6.000 mm
- Poids (cts)
- 81.940
- Taper
- Rough
- Couleurs
-
[SAME TREATMENT APPLIES TO FAIRY OPAL]
This is a natural opal treated so it becomes black- We purchase large quanites of rough material and slab it and then treat it so you can get a idea of how it will face. There is a large amount of wastage in preparing this material. You can cut into earrings ring or pendant stones or leave as specimens but you will have to re treat if you take too much away. Check that there isnt another colour bar in the rough you cant expose that may be better than the top.
You may see black spots which is usually blackened sugar which will come off.
Mined in Andamooka Sth Australia
We havve taken the photo of the rough wet!
TREATMENT FOR ANDAMOOKA MATRIX WITH SUGAR ONLY.
MATERIALS
250 grams glucose,white castor sugar,pot or pressure cooker,plastic tweezers.
STEPS
-Pre shape the material
- Thoroughly dry the material in oven sun or hairdryer. You can also soak in aceton for 10 minutes to dry the stones out.
- Put water in pot on low temperature and add glucose and castor sugar. DO NOT BOIL.
-Place warmed stones into warm solution and cover the stone with liquid.
-leave on low temperature for 24 hours but DONT BOIL.
-Remove with tweezers and let cool.Use a paper town to wipe away access.
The next steep is to carbonize the sugar in the stone. Place the stones on a metal or pyrex dish and place in a kiln at 500 F degrees for one hour.This will burn or carbonize the sugar in the stone.
_When the stones have cooled clean on a grinding wheel.
Remember to take all precautions with gloves and mask and clothing with good ventilation.
This is a natural product so results may vary a bit due to how porous the sandstone is. Some material will have to be treated a few times to get good results. You can also experiment with various temperatures as i like to cook with lower temperatures.
Remember to have fun!
WE HAVE TAKEN THE PHOTO WITH THE ROUGH WET.
In the learning section of opal actions there is details on how to treat with acid and sugar but this sugar only gets good results if the material is porous
-
POLISHING
The surface is porous so its hard to get a good finish.
You can polish as a natural stone or coat it with resin to get a better finish.
We suggest a polymer resin as its stable.inert and nontoxic and dosent yellow..Check out our listings of fairy opal polished in sedaopals.Some of there were polished in china under vacume with a amazing finish.
We have also used mono-compontent thermo set resin,cynoacrylates and 2 parts resin but these can turn yellow over time. ive even heard of nail polished used and hardened under uv lights.
The weight and size is app
Fournisseur d'expédition | Expédition vers :pays | Expédition dans le reste du monde |
---|---|---|
FedEx | $12.00 / : jours jours | $39.00 / : jours jours |
:pays
:fournisseur bénéficie d'une réduction de :prix sur les commandes avec :quantité ou plus d'articles
Reste du monde
:fournisseur bénéficie d'une réduction de :prix sur les commandes avec :quantité ou plus d'articles
|
||
Express Shipping | $12.00 / : jours jours | $39.00 / : jours jours |
:pays
:fournisseur bénéficie d'une réduction de :prix sur les commandes avec :quantité ou plus d'articles
Reste du monde
:fournisseur bénéficie d'une réduction de :prix sur les commandes avec :quantité ou plus d'articles
|
||
Registered Shipping | $9.00 / : jours jours | $16.00 / : jours jours |
:pays
:fournisseur bénéficie d'une réduction de :prix sur les commandes avec :quantité ou plus d'articles
Reste du monde
:fournisseur bénéficie d'une réduction de :prix sur les commandes avec :quantité ou plus d'articles
|
-
Positif
Paid and shipped - no feedback left after 100 days
-
Positif
Fast as lightning shipping and delivery. Great vendor to deal with and I'll definitely be back for another visit.
-
Positif
Great selection of stones, found myself a couple of beautiful little pieces in there auction category. Super fast shipping and delivery. A+ vendor
Pourquoi les utilisateurs se surenchérissent-ils ?
Lorsqu'une enchère est placée, il s'agit du montant maximum qu'un utilisateur est prêt à enchérir pour le produit. Notre système enchérira ensuite automatiquement au nom de cet utilisateur, augmentant progressivement l'enchère pour maintenir sa position d'enchérisseur le plus élevé, jusqu'au maximum spécifié.
Lorsqu'il y a une icône indiquant "Enchère automatique", cela signifie que notre système place activement des enchères pour l'utilisateur en fonction de son enchère maximale. Cela peut donner l'impression que les utilisateurs surenchérissent eux-mêmes, mais c'est simplement le résultat de la mise à jour de l'enchère par le système pour refléter la limite maximale des utilisateurs.